Hongji Helps You Find the Cause of Shifting Sand Material


Shifting sand, also known as sticky bulk material, the surface was dark green, but the end grain is very poor, it was powder state. Hongji experts told reporters, shifting sand material will seriously affect the operation rate of the kiln skin, damage to bricks and kiln, increase production costs and affect the production efficiency.
rotary kiln

In the production process of rotary kiln, what are the causes for shifting sand material returned?
Due to operational errors, causing the imbalance of wind, coal, matching material, preheater, calciner and burning zone and other parts, serious damage to the firing system, thermal system, leading to the formation of black clinker.
In addition, if rotary kiln occurs ring forming without timely treatment, resulting in material stays in the firing zone for a long time, the material layer of burning zone is relatively thick.
Frequent shifting sand phenomenon, caused great damage to the brick, replace bricks at least to stop the kiln 24h, increase production costs and affect the production schedule, caused great economic losses to the enterprise.
After eliminating the phenomenon of shifting sand, the operating efficiency of rotaey kiln has been significantly improved. The yield of rotary kiln has been improved significantly, to create greater economic benefits for enterprises.
Glitch brings big impact, Hongji machine reminds that users donot ignore a small problem, find and solve problems, Hongji provides you with a full range of services, please call us for more information.zrf